Rubber RTV-2 GI-1040 Silicones, Inc.
0
Technical Data Sheet
| Cured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | ASTM D412 | 3.45to3.79 MPa | |
| elongation | Break | ASTM D412 | 200to250 % |
| tear strength | ASTM D624 | 14.9to20.1 kN/m | |
| Coverage-Cured | 0.910 cm³/g | ||
| Shore hardness | ShoreA4 | 26to34 | |
| ShoreA5 | 36to44 |
| Uncured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Color | --2 | Blue | |
| --3 | OffWhite | ||
| viscosity | --2 | 0.30to0.40 Pa·s | |
| --3 | 90to110 Pa·s | ||
| 固化时间 | 16to18 hr | ||
| Pot Life | 90to150 min |
| thermosetting | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Thermosetting components | Shelf Life | 26 wk | |
| 热固性混合粘度 | 50000to65000 cP | ||
| Resin | 按容量计算的混合比:100按重量计算的混合比:10 | ||
| Hardener | 按容量计算的混合比:11按重量计算的混合比:1.0 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Usage temperature | 固化后 | -51-177 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | 1.10 g/cm³ | ||
| Shrinkage rate | 固化后 | 0.20 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.