PP+EPDM TPV 40D 1070

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityDIN535050.940 g/cm³
hardnessTest ConditionTest MethodTest Result
DIN5350540
elastomerTest ConditionTest MethodTest Result
Tensile stress flow rateYieldDIN5350516.0 MPa
BreakDIN53505630 %
DIN5350580 kN/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.