Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ASTMD955 | 0.40到0.60 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 92 |
Rockwell hardness | | ASTMD785 | 124 |
optical performance | Test Condition | Test Method | Test Result |
---|
transmissivity | | ASTMD1003 | 88.0 % |
Yellowness Index | | ASTMD1925 | 40 YI |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Dart impact equipped with measuring instruments | | ASTMD3763 | 68.0 J |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 1900 Mpa |
tensile strength | | ASTMD638 | 83.0 Mpa |
tensile strength | | ASTMD638 | 69.0 Mpa |
elongation | | ASTMD638 | 9.0 % |
elongation | | ASTMD638 | 30 % |
Flexural modulus | | ASTMD790 | 2300 Mpa |
bending strength | | ASTMD790 | 97.0 Mpa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 132 °C |
| | ASTMD648 | 143 °C |
| | ASTMD648 | 116 °C |
| | ASTMD648 | 138 °C |
vicat | | ASTMD1525 | 147 °C |
| | ASTMD696 | 5.8E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.