PA6 PAmpellonne® 601s

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO11831.13到1.14 g/cm³
Ash ContentISO3451-40.30到0.50 %
humidityISO15512/B0.10到0.30 %
relative viscosity2.60到2.80
hardnessTest ConditionTest MethodTest Result
ISO86875到85
Supplementary InformationTest ConditionTest MethodTest Result
DSCAnalysis>96 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile strainBreakISO527-2>5.0 %
Tensile modulusISO527-23000到4000 MPa
Tensile stressYieldISO527-280.0到90.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO179/1A5.0到7.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
ISO3146220到225 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.