Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D1238 | 0.40 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTM D2457 | 100 |
Haze ratio | | ASTM D1003 | 7.0 % |
other | Test Condition | Test Method | Test Result |
---|
characteristic | | | 薄膜级 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
Viscosity | | ASTM D3354 | 20.0 g/100cm² |
Content of lubricant | | 内部方法 | 0.900 Tanθ |
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D-1238 | 0.4 g/10min |
density | | ASTM D-792 | 0.921 g/cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTM D638 | 19.6 Mpa |
elongation | | ASTM D638 | 700 % |
Flexural modulus | | ASTM D747 | 210 Mpa |
tensile strength | | ASTM D-638 | 200 kg/cm |
elongation | | ASTM D-638 | 700 % |
elongation at break | | ASTM D638/ISO 527 | 700 % |
tensile strength | | ASTM D638/ISO 527 | 19.6 kg/cm²(MPa)[Lb/in²] |
Other performance | Test Condition | Test Method | Test Result |
---|
rigid | | ASTM D-747 | 2100 kg/cm |
rigid | | ASTM D-747 | 2100 °C |
film | Test Condition | Test Method | Test Result |
---|
film thickness | | | 30 µm |
Physical properties | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792/ISO 1183 | 0.921 |
melt mass-flow rate | | ASTM D1238/ISO 1133 | 0.4 g/10min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | 内部方法 | 109 °C |
melting temperature | | | 109 ℃(℉) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.