Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D-792 | 1.22 g/cm³ | |
water content | 内部方法 | < 0.10 % | |
Shore hardness | Shore A | ASTM D-2240 | 94 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D-412 | 11.0 MPa | |
Yield | ASTM D-412 | 35.0 MPa | |
elongation | Break | ASTM D-412 | 500 % |
tear strength | ASTM D-624 | 120 kN/m | |
Wear amount | DIN 53516 | 25.0 mm³ |
squeeze out | Test Condition | Test Method | Test Result |
---|---|---|---|
drying temperature | 98.9 to 110 ℃ | ||
drying time | 1.0 to 2.0 hr | ||
auxiliary word for ordinal numbers | 152 to 179 ℃ | ||
163 to 191 ℃ | |||
171 to 202 ℃ | |||
177 to 204 ℃ | |||
Temperature | 177 to 199 ℃ |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Glass Transition Temperature | DIN 51007 | -13.9 ℃ | |
melting temperature | 内部方法 | 199 to 210 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.