Technical Data Sheet
other | Test Condition | Test Method | Test Result |
---|---|---|---|
notes | 经济型 易加工 |
processability | Test Condition | Test Method | Test Result |
---|---|---|---|
Dry conditions | 80度-90度 3-4小时 | ||
process temperature | 185 °C | ||
175 °C | |||
180 °C | |||
185-195 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
100% modulus | ASTM D412/ISO 527 | 80 Mpa/Psi | |
300% modulus | ASTM D412/ISO 527 | 120 Mpa/Psi | |
tear strength | ASTM D624/ISO 34 | 140 n/mm² | |
ASTM D2240/ISO 868 | 90 Shore A | ||
Hardness D | ASTM D2240/ISO 868 | 39 Shore D | |
Abrasion loss | ISO 4649 | 100 mm³ | |
ISO 815 | 35 % |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792/ISO 2781/JIS K7311 | 1.23 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.