PPS TS201HS TOYOBO JAPAN
57
Form:Granules | Grade:Injection grade
Properties:
dimensional stability High rigidityFiller: Glass mineral
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | dimensional stability | High rigidity | Filler: Glass mineral |
Certificates
No Data...
Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| characteristic | 玻璃纤维和无机物填充增强等级.与40%玻璃纤维增强等级一样的性能 | |||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | V-0 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ASTM D790/ISO 178 | 21*10^4 | kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 2650 | kg/cm²(MPa)[Lb/in²] | |
| tensile strength | ASTM D638/ISO 527 | 2010 | kg/cm²(MPa)[Lb/in²] | |
| Tensile modulus | ASTM D638/ISO 527 | 23*10^4 | kg/cm²(MPa)[Lb/in²] | |
| bending strength | Yield | ASTM D790 | 234 | Mpa |
| Bending modulus | ASTM D790 | 18600 | Mpa | |
| elongation | Break | ASTM D638 | 1.4 | % |
| tensile strength | Yield | ASTM D638 | 170 | Mpa |
| Tensile modulus | ASTM D638 | 21600 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | TD | ASTM D696 | 4.8E-05 | cm/cm/°C |
| MD | ASTM D696 | 1.2E-05 | cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 260 | °C |
| HDT | ASTM D648/ISO 75 | >260 | ℃(℉) | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 24hr | ASTM D570 | 0.020 | % |
| Shrinkage rate | TD | ASTM D955 | 0.45 | % |
| MD | ASTM D955 | 0.15 | % | |
| density | ASTM D792/ISO 1183 | 1.96 | ||
| Water absorption rate | ASTM D570/ISO 62 | 0.02 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Arc resistance | ISO 14782 | 173 | ||
| Dissipation factor | 1MHz | ASTM D150 | 8.5E-03 | |
| 1kHz | ASTM D150 | 0.055 | ||
| Dielectric constant | 1MHz | ASTM D150 | 4.50 | |
| 1kHz | ASTM D150 | 5.10 | ||
| Dielectric strength | ASTM D149 | 11 | KV/mm | |
| Volume resistivity | ASTM D257 | 1E+15 | ohms·cm | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 3 | ||
| Arc resistance | ASTM D495 | 137 | sec | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 121 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.