Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
VA content | HYUNDAI | 3 % | |
gloss | ASTM D-2457 | 85 | |
film thickness | HYUNDAI | 50 um | |
Haze ratio | ASTM D-1003 | 5.6 % |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D-1505 | 0.926 g/cm | |
melt mass-flow rate | ASTM D-1238 | 0.60 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strength at break | ASTM D-882 | 300 kg/cm | |
Falling ball impact strength | ASTM D-1709 | 270 g | |
elongation at break | ASTM D-882 | 500 % | |
ASTM D-882 | 660 % | ||
Tensile strength at break | ASTM D-882 | 330 kg/cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.