Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
密度 | | ASTMD792 | 0.877 g/cm³ |
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 15 g/10min |
机械性能 | Test Condition | Test Method | Test Result |
---|
拉伸模量- | Compression Molded | ASTMD638 | 2.31 MPa |
抗张强度 | 断裂,模压成型 | ASTMD638 | 7.00 MPa |
伸长率 | 断裂,模压成型 | ASTMD638 | 1500 % |
弹性体 | Test Condition | Test Method | Test Result |
---|
压缩永久变形 | 70°C | ASTMD395 | 58 % |
抗张强度 | Break | ASTMD412 | 7.00 MPa |
伸长率 | Break | ASTMD412 | 1700 % |
撕裂强度 | | ASTMD624 | 31.0 kN/m |
压缩永久变形 | 21°C | ASTMD395 | 15 % |
硬度 | Test Condition | Test Method | Test Result |
---|
肖氏硬度 | 邵氏A,模压成型 | ASTMD2240 | 71 |
热性能 | Test Condition | Test Method | Test Result |
---|
溶融温度 | | 内部方法 | 120 °C |
TMA | 1.00mm | 内部方法 | 95 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.