TPU-Ester Zythane® 4065D

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.23 g/cm³
hardnessTest ConditionTest MethodTest Result
ASTMD224064
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94HB
UL flame retardant ratingUL94HB
UL flame retardant ratingUL94HB
Mechanical propertiesTest ConditionTest MethodTest Result
ASTMD104445.0 mg
Abrasion-DINDIN5351650 mm³
elastomerTest ConditionTest MethodTest Result
compression setASTMD395B48 %
elongationBreakASTMD412340 %
tear strengthASTMD624137 kN/m
compression setASTMD395B38 %
Tensile stressASTMD41220.0 MPa
Tensile stressASTMD41240.0 MPa
tensile strengthBreakASTMD41255.0 MPa
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureDSC-5.00 °C
vicatASTMD1525162 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.