plas
Log In

PUR-PC M 3900 CHEMTURU USA

0

Technical Data Sheet

Uncured PropertiesTest ConditionTest MethodTest Result
Curing time115°C1.0 hr
elastomerTest ConditionTest MethodTest Result
Shore hardnessASTM D263237 %
Permanent compression deformation70°C,22hrASTM D395B37 %
tear strengthSplitASTM D47023 kN/m
tear strength--2ASTM D624111 kN/m
elongationBreakASTM D412260 %
tensile strengthASTM D41238.7 MPa
tensile strength100%StrainASTM D41215.3 MPa
mechanical propertiesTest ConditionTest MethodTest Result
compressive strength25%StrainASTM D69513.1 MPa
compressive strength20%StrainASTM D6959.45 MPa
compressive strength15%StrainASTM D6957.03 MPa
compressive strength10%StrainASTM D6954.41 MPa
compressive strength5%StrainASTM D6951.45 MPa
thermosettingTest ConditionTest MethodTest Result
Post curing time115°C16 hr
storage stability1.5 min
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreAASTM D224096to97
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.