PMMA CP-71 Lucite (Taiwan)
0
- Properties:Electrical insulationgood chemical corrosion resistancegood impact resistancegood processing performancegood dimensional stabilitygood weather resistancehigh clarityhigh heat resistancelow to odorlesslow to tastelessprocessablemedium flow ratemedium molecular weight
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.19 g/cm | |
Shrinkage rate | ASTM D955 | 0.5 % | |
Rockwell hardness | ASTM D785 | 90 |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
refractive index | ASTM D542 | 1.49 | |
transmittance | ASTM D1003 | 92 % | |
Haze ratio | ASTM D1003 | 1 % |
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | ASTM D570 | 0.3 % | |
melt mass-flow rate | ASTM D1238 | 3.9 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Dart impact | ASTM D3029 | 0.339 J | |
bending strength | ASTM D790 | 101 MPa | |
Tensile modulus | ASTM D638 | 3240 MPa | |
tensile strength | ASTM D638 | 67.6 MPa | |
elongation | Break | ASTM D638 | 3.1 % |
Flexural modulus | ASTM D790 | 3080 MPa | |
Impact strength of cantilever beam gap | ASTM D256 | 21.4 J/m | |
Suspended wall beam without notch impact strength | ASTM D256 | 283 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 96.7 ℃ | |
vicat | ASTM D1525 | 107 % | |
Linear coefficient of thermal expansion | ASTM D696 | 0.000061 cm/cm/℃ | |
UL flame retardant rating | UL 94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.