PA6 LUBEMID B27 GF25 NATURAL
0
- Properties:Fillerglass fiber reinforced material25%filler by weight
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO1183/A | 1.29到1.33 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Burning wire flammability index | IEC60695-2-12 | 650 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO527-2/1A/1 | 7500到8000 MPa | |
Tensile stress | Yield | ISO527-2/1A/5 | 125到135 MPa |
Break | ISO527-2/1A/5 | 125到135 MPa | |
Tensile strain | Yield | ISO527-2/1A/5 | 2.0到3.0 % |
Break | ISO527-2/1A/5 | 2.0到3.0 % | |
Flexural modulus | ISO178 | 7000到7500 MPa | |
Bending stress | ISO178 | 165到175 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTMD256 | 60到70 kJ/m² | |
ASTMD256 | 8.0到9.0 kJ/m² | ||
ISO180/A | 7.0到8.0 kJ/m² | ||
ISO180 | 50到60 kJ/m² | ||
Charpy Notched Impact Strength | ISO179/1eA | 7.0到8.0 kJ/m² | |
Impact strength of simply supported beam without notch | ISO179/1eU | 50到60 kJ/m² | |
Impact strength of cantilever beam gap | ASTMD256A | 80到90 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD648 | 210到220 °C | ||
ISO75-2/B | 215到225 °C | ||
ASTMD648 | 200到210 °C | ||
vicat | ISO306/A120 | 210到220 °C | |
ISO306/B120 | 205到215 °C | ||
melting temperature | 内部方法 | 210到225 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.