Share
Add to Compare

PP 9C19300 FR3 4Plas

Properties:
Characteristics conductivity copolymer
Product Description
Certificates(0)
Datasheet

Product Description

Properties:Characteristics | conductivity | copolymer

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°CISO 180/1A60kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU无断裂
Impact strength of simply supported beam without notch-30°CISO 179/1eU无断裂
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.6mmUL 94V-2
UL flame retardant rating1.60 mmUL 94V-2
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
tensile strengthBreak,23°CISO 527-2/525.0MPa
Tensile modulus23°CISO 527-2/51250MPa
Impact strength of simply supported beam without notch23°CISO 179/1eU无断裂
tensile strengthBreak, 23°CISO 527-2/525MPa
Tensile modulus23°CISO 527-2/51250MPa
Impact strength of cantilever beam gap23°CISO 180/1A60kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU无断裂
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Melting temperatureISO 11357160°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A50.0°C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B90.0°C
Hot deformation temperature1.8 MPa, UnannealedISO 75-2/A50°C
Hot deformation temperature0.45 MPa, UnannealedISO 75-2/B90°C
Melting temperatureISO 11357160°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate230°C/2.16kgISO 11336.0g/10min
densityISO 11830.990g/cm³
melt mass-flow rate230°C/2.16 kgISO 11336.0g/10 min
densityISO 11830.990g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Volume resistivityIEC 60093< 1.0E+4ohms·cm
Surface resistivityIEC 60093< 1.0E+4ohms
Volume resistivityIEC 60093<1.0E+4ohms·cm
Surface resistivityIEC 60093<1.0E+4ohms
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.