| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C,12.7mm | ASTM D256 | 230 | J/m |
| 23°C,3.20mm | ASTM D256 | 270 | J/m | |
| 0°C,12.7mm | ASTM D256 | 180 | J/m | |
| 0°C,3.20mm | ASTM D256 | 200 | J/m | |
| -30°C,12.7mm | ASTM D256 | 120 | J/m | |
| -30°C,3.20mm | ASTM D256 | 140 | J/m | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 20 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| --5 | ISO 178 | 78.0 | Mpa | |
| --4 | ASTM D790 | 74.0 | Mpa | |
| Bending modulus | ASTM D790 | 2280 | Mpa | |
| crack | ISO 527-2/50 | >10 | % | |
| ASTM D638 | 48 | % | ||
| yield | ISO 527-2/50 | 51.0 | Mpa | |
| ASTM D638 | 48.0 | Mpa | ||
| Tensile modulus | ISO 527-2/1 | 2600 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 7.4E-05 | cm/cm/°C |
| thermal conductivity | ASTMC177 | 0.15 | W/m/K | |
| 1.8MPa, unannealed | ISO 75-2/A | 83.0 | °C | |
| 1.8MPa, unannealed, 12.7mm | ASTM D648 | 93.0 | °C | |
| 1.8MPa, unannealed, 6.40mm | ASTM D648 | 88.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23°C,24hr | ASTM D570 | 0.30 | % |
| Shrinkage rate | MD | ASTM D955 | 0.40-0.60 | % |
| melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 15 | g/10min |
| density | ASTMD792 | 1.04 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ASTM D257 | >1.0E+16 | ohms | |
| Volume resistivity | 23°C | ASTM D257 | >1.0E+16 | ohms·cm |
| Dielectric strength | ASTM D149 | 23 | KV/mm | |
| Dielectric constant | 1kHz | ASTM D150 | 3.10 | |
| Dissipation factor | 1kHz | ASTM D150 | 6.6E-03 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Scale | ASTM D785 | 112 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.