HDPE Alathon®  L5040TC

7
  • Properties:
    High toughness
    Easy to process
    High rigidity
  • Usages:
    catheter
    Wire and cable
    Communication equipment

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateASTMD12380.39 g/10min
Resistance to environmental stress crackingASTMD1693B>96.0 hr
Resistance to environmental stress crackingASTMD1693B>1000 hr
hardnessTest ConditionTest MethodTest Result
ASTMD224063
Supplementary InformationTest ConditionTest MethodTest Result
CellClassificationASTMD3350435580A
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63824.8 Mpa
elongationASTMD638>600 %
ASTMD790951 Mpa
Impact resistanceTest ConditionTest MethodTest Result
TensileImpactASTMD1822100 J/cm
Thermal performanceTest ConditionTest MethodTest Result
ASTMD64876.0 °C
brittle temperatureASTMD746<-75.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.