POM HC750 ASAHI JAPAN
166
Form:Granules | Grade:Injection grade
Properties:
copolymerHigh mobility
Typical Applications:
Automotive sectorElectrical fieldElectronic fieldHousehold goodsIndustrial applications
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Automotive sector | Electrical field | Electronic field | Household goods | Industrial applications |
| Properties: | copolymer | High mobility |
Certificates

Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Water absorption rate | 24 hr | ASTM D570 | 0.2 | % |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ASTM D638/ISO 527 | 3200(MPa) | kg/cm²(MPa)[Lb/in²] | |
| elongation | Break | ISO 527-2 | 45 | % |
| bending strength | ASTM D790 | 98 | MPa | |
| Impact strength of cantilever beam gap | ASTM D256 | 59 | J/m | |
| Tensile modulus | ISO 527-2 | 3200 | MPa | |
| Tensile stress | Yield | ISO 527-2 | 71 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Combustibility (rate) | UL 94 | HB | ||
| Hot deformation temperature | 0.45MPa,unannealed | ASTM D648 | 163 | ℃ |
| 1.8MPa,unannealed | ASTM D648 | 124 | ℃ | |
| 1.8MPa,unannealed | ISO 75-2/A | 107 | ℃ | |
| UL flame retardant rating | UL 94 | HB | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792/ISO 1183 | 1.41 | ||
| Shrinkage rate | ASTM D955 | 1.6-2.0 | % | |
| Flow | ASTM D955 | 1.6-2 | % | |
| Across Flow | ISO 294-4 | 1.6-2 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.