Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:1.0按容量计算的混合比:1.0 |
| | | 按重量计算的混合比:1.0按容量计算的混合比:1.1 |
| | | 52 wk |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
colour | | | Colorless |
colour | | | Grey |
density | | | 1.31 g/cm³ |
density | | | 1.38 g/cm³ |
| | ASTMD2393 | 2.0 Pa·s |
| | ASTMD2393 | 2.0 Pa·s |
| | ASTMD2393 | 2.0 Pa·s |
Curing Time | | | 0.25 hr |
Curing Time | | | 1.0 hr |
Curing Time | | | 4.0 hr |
Curing Time | | | 24 hr |
Curing Time | | | 2.4E+2到3.6E+2 min |
Curing Time | | | 60到90 min |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | ASTMD2240 | 52到58 |
elastomer | Test Condition | Test Method | Test Result |
---|
tear strength | | ASTMD624 | 3.15 kN/m |
tensile strength | | ASTMD412 | 3.45 MPa |
elongation | Break | ASTMD412 | 140 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTMD257 | 1.5E+15 ohms·cm |
dielectric strength | | ASTMD149 | 22 kV/mm |
dielectric constant | | ASTMD150 | 3.00 |
Dissipation Factor | | ASTMD150 | 7E-03 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | | 2.2E-04 cm/cm/°C |
thermal conductivity | | | 0.31 W/m/K |
Service | | | -55到204 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.