Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | 内部方法 | 4.0 % |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
not transparent | BS4432 | 64 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Itself - Dynamic | ASTMD1894 | 0.30 | |
Itself - Static | ASTMD1894 | 0.35 |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Sealing emphasis | 内部方法 | 0.14 N/mm | |
内部方法 | 116到146 °C | ||
oxygen permeability | ASTMF1927 | 41 cm³·mm/m²/atm/24hr | |
Water vapor permeability | ASTMF1770 | 5.0 g/m²/24hr | |
CoronaTreatment | 内部方法 | 38 dyne/cm | |
film thickness | 内部方法 | 120 | |
usage | 内部方法 | 34.1 m²/kg |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.