Technical Data Sheet
Test Condition | Test Method | Test Result | |
---|---|---|---|
yield | 1.03to33.45 Mpa | ||
Nominal tensile fracture strain | % | 2.5to500 | |
fracture | 14.0to64.0 Mpa | ||
yield | 4.0to51.03 Mpa | ||
transmissivity | % | 88.9to93.1 | |
fracture | % | 550to850 | |
yield | 1.7to33.03 Mpa | ||
fracture | % | 400to890 | |
Haze ratio | % | 0.20to3.1 | |
Maximum continuous use temperature | °C | 150to170 | |
burning rate | mm/min | 38.1to53.34 | |
brittle temperature | °C | -60--59 | |
Heat distortion temperature | °C | 59to62 | |
Impact strength of cantilever beam gap | J/m | 0.007to0.037 | |
Dart impact | N.m | 47.17to3256.64 | |
Charpy Notched Impact Strength | kJ/m² | 0.353to2.182 | |
yield | % | 2.0to2.1 | |
compression set | % | 18to36 | |
fracture | 3.97to20.34 Mpa | ||
yield | 24.41to54.0 Mpa | ||
Melt volume flow rate | cm³/10min | 0.04to0.05 | |
flow | mm/mm | 152.4E-3-172.7E-3 | |
fracture | % | 30to260 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top