HMW-HDPE Kemcor HD 2470 Ixom Operations Pty Ltd
0
- Properties:Mechanical properties
- Usages:Pipeline system
Technical Data Sheet
Test Condition | Test Method | Test Result | |
---|---|---|---|
抗张强度 | Yield | ASTMD638 | 24.0 MPa |
Break | ASTMD638 | 30.0 MPa | |
伸长率 | Break | ASTMD638 | 800 % |
弯曲模量 | ASTMD790 | 970 MPa | |
熔融温度 | 130 °C | ||
线性热膨胀系数 | MD | ASTMD696 | 1.4E-04 cm/cm/°C |
密度 | ASTMD1505 | 0.956 g/cm³ | |
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 0.10 g/10min |
肖氏硬度 | 邵氏D | ASTMD2240 | 63 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.