PC 261-3 STYRON US
11
Form:Granules | Grade:Injection grade
Properties:
transparentheat-resistingHigh impact resistanceExcellent heat resistanceGood transparency and ext
Typical Applications:
Food containerscontainerLarge food containers
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Food containers | container | Large food containers |
| Properties: | transparent | heat-resisting | High impact resistance | Excellent heat resistance | Good transparency and ext |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | ASTM D542 | 1.586 | ||
| Transmittance rate | ASTM D1003 | 89 | % | |
| turbidity | ASTM D1003 | 0.7-1.5 | % | |
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
| Limiting Oxygen Index (LOI) | ASTM D2863 | 26 | % | |
| Average degree of combustion | ASTM D638 | 25 | mm | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ASTM D638 | 2480 | Mpa | |
| bending strength | ASTM D790 | 96 | Mpa | |
| Bending modulus | ASTM D790 | 2410 | Mpa | |
| Impact strength of cantilever beam gap | ASTM D256 | 950 | J/m | |
| tensile strength | Yield | ASTM D638 | 60 | Mpa |
| Rockwell hardness | ASTM D785 | 74 | M | |
| tensile strength | Break | ASTM D638 | 72 | Mpa |
| elongation at yield | ASTM D638 | 6 | % | |
| Elongation at Break | ASTM D638 | 150 | % | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | Annealed,0.45Mpa | ASTM D648 | 146 | °C |
| Annealed,1.8Mpa | ASTM D648 | 143 | °C | |
| Unannealed,1.8Mpa | ASTM D648 | 143 | °C | |
| Vicat softening temperature | ASTM D1525 | 151 | °C | |
| Linear coefficient of thermal expansion | ASTM D696 | 68 | ×10 | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.2 | ||
| Shrinkage rate | ASTM D955 | 0.005-0.007 | mm/mm | |
| Water absorption rate | 23℃,24H | ASTM D570 | 0.15 | % |
| 23℃,50%相对湿度 | ASTM D570 | 0.32 | % | |
| melt mass-flow rate | ASTM D1238 | 2.6 | g/10min | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Glow wire combustion index (GWFI) | IEC 695-2-1 | 850 | °C | |
| Compared to the Leakage Traceability Index (CTI) | IEC 112 | 250 | V | |
| Dielectric strength | ASTM D149 | 17 | KV/mm | |
| Volume resistivity | ASTM D257 | 2×10 | Ω.cm | |
| Dissipation factor | ASTM D150 | 3 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.