Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTMD1238 | 7.0 g/10min |
Shrinkage rate | | ASTMD955 | 0.50到0.70 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 123 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating 3 | | UL94 | V-0 |
UL flame retardant rating 3 | | UL94 | V-0 |
Burning wire flammability index 4 | | IEC60695-2-12 | 960 °C |
Extreme Oxygen Index 5 | | ASTMD2863 | 35 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
elongation | | ASTMD638 | 110 % |
Flexural modulus | | ASTMD790 | 2400 Mpa |
bending strength | | ASTMD790 | 93.8 Mpa |
Tensile modulus | | ASTMD638 | 2210 Mpa |
tensile strength | | ASTMD638 | 60.0 Mpa |
tensile strength | | ASTMD638 | 57.9 Mpa |
elongation | | ASTMD638 | 6.2 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Dart impact equipped with measuring instruments 1 | | ASTMD3763 | 58.8 J |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 139 °C |
| | ASTMD648 | 127 °C |
vicat | | ASTMD15252 | 149 °C |
| | ASTMD696 | 6.5E-05 cm/cm/°C |
RTI Elec | | UL746 | 125 °C |
RTI Imp | | UL746 | 125 °C |
RTI | | UL746 | 125 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.