TPEE HYT3078 BK176 DUPONT USA
107
Form:Granules | Color:black | Grade:Toughened grade
Properties:
Toughening
Typical Applications:
Keys
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Keys |
| Properties: | Toughening |
| Color: | black |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak | |
| -30°C | ISO 179/1eU | NoBreak | ||
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Burning rate | 1.00mm | ISO 3795 | <100 | mm/min |
| UL flame retardant rating | 1.5mm | UL 94 | HB | |
| 3.0mm | UL 94 | HB | ||
| 1.5mm | IEC 60695-11-10,-20 | HB | ||
| 3.0mm | IEC 60695-11-10,-20 | HB | ||
| Extreme Oxygen Index | ISO 4589-2 | 19 | % | |
| FMVSS flammability | FMVSS302 | B | ||
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
| tear strength | Flow | ISO 34-1 | 80 | kN/m |
| 横向Flow | ISO 34-1 | 77 | kN/m | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 21.0 | Mpa | |
| Tensile creep modulus | 1000hr | ISO 899-1 | 18.0 | Mpa |
| 1hr | ISO 899-1 | 22.0 | Mpa | |
| Nominal tensile fracture strain | ISO 527-2 | 900 | % | |
| Tensile strain | Break | ISO 527-2 | >300 | % |
| tensile strength | 50%Strain | ISO 527-2 | 5.00 | Mpa |
| 10%Strain | ISO 527-2 | 1.80 | Mpa | |
| Break | ISO 527-2 | 24.0 | Mpa | |
| Tensile modulus | ISO 527-2 | 24.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Glass transition temperature | ISO 11357-2 | -60.0 | °C | |
| Brittle temperature | ISO 974 | -98.0 | °C | |
| Melting temperature | ISO 11357-3 | 177 | °C | |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.8E-04 | cm/cm/°C |
| TD | ISO 11359-2 | 2.1E-04 | cm/cm/°C | |
| Effective thermal diffusivity coefficient | 5.44E-08 | m²/s | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,2.00mm,50%RH | ISO 62 | 0.20 | % |
| Saturation,23°C,2.00mm | ISO 62 | 0.80 | % | |
| 23°C,24hr | ISO 62 | 0.50 | % | |
| Shrinkage rate | MD | ISO 294-4 | 0.60 | % |
| TD | ISO 294-4 | 0.60 | % | |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 5.00 | cm3/10min |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 5.0 | g/10min |
| MediumDensity | 0.940 | g/cm³ | ||
| SpecificHeatCapacity of Melt | 2150 | J/kg/°C | ||
| ThermalConductivityofMelt | 0.15 | W/m/K | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dissipation factor | 1MHz | IEC 60250 | 0.015 | |
| Surface resistivity | IEC 60093 | 1E+14 | ohms | |
| Volume resistivity | IEC 60093 | 1E+13 | ohms·cm | |
| Dielectric strength | IEC 60243-1 | 18 | KV/mm | |
| Relative permittivity | 100Hz | IEC 60250 | 5.40 | |
| 1MHz | IEC 60250 | 5.30 | ||
| Dissipation factor | 100Hz | IEC 60250 | 7E-03 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD,15Sec | ISO 868 | 26 | |
| ShoreD | ISO 868 | 30 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.