Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Apparent density | JISK6891 | 0.75到1.05 | g/cm³ | |
Melt mass flow rate | 372°C/5.0kg | ASTMD3307 | 5.0到7.0 | g/10min |
Particle size | 150到250 | µm |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | 邵氏D | ASTMD2240 | 60 | |
tensile strength | JISK6888 | 19.6到31.4 | Mpa | |
elongation | 断裂 | JISK6888 | 250到350 | % |
friction coefficient | 与自身-静态 | 内部方法 | 0.050到0.080 | |
Taber abraser | CS-17转轮 | 5.00到15.0 | mg |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melting temperature | ASTMD3307 | 303到313 | °C |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Adhesion Strength PeelTest | 4.0到6.0 | kN/m | ||
Contact Angle | Hexadecane | 65.0 | ° | |
Water | 102到106 | ° |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.