PEEK Larpeek 50 G/30

0
  • Properties:
    Filler
    glass fiber reinforced material
    30%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11831.50 g/cm³
Shrinkage rateISO 294-40.60to0.90 %
Shrinkage rateISO 294-40.25to0.50 %
Water absorption rateISO 620.060 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-1
UL flame retardant ratingUL 94V-0
UL flame retardant ratingUL 94V-0
Burning wire flammability indexIEC 60695-2-12960 °C
Hot filament ignition temperatureIEC 60695-2-13875 °C
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/110500 MPa
Tensile modulusISO 527-2/110500 MPa
tensile strength ISO 527-2/5175 MPa
tensile strength ISO 527-2/5160 MPa
tensile strength ISO 527-2/5155 MPa
tensile strength ISO 527-2/5135 MPa
tensile strength ISO 527-2/5110 MPa
Tensile strainISO 527-2/52.2 %
Tensile strainISO 527-2/52.2 %
Tensile strainISO 527-2/52.2 %
Tensile modulusISO 527-2/111500 MPa
Tensile strainISO 527-2/52.3 %
Tensile strainISO 527-2/52.4 %
Tensile modulusISO 527-2/111500 MPa
Tensile modulusISO 527-2/111000 MPa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 179/1eA10 kJ/m²
Impact strength of simply supported beam without notchISO 179/1eU70 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
vicatISO 306/B50>300 °C
Linear coefficient of thermal expansionISO 11359-21.5E-05 cm/cm/°C
Heat distortion temperatureISO 75-2/B>300 °C
Heat distortion temperatureISO 75-2/A>300 °C
Continuous use temperature230 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.