Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| | | 按重量计算的混合比:80,按容量计算的混合比:68 |
| | | 按重量计算的混合比:100,按容量计算的混合比:100 |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792,ASTMD1622 | 1.04 g/cm³ |
Shrinkage rate | | 内部方法 | 0.80到0.90 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 94 |
| | ASTMD2240 | 45 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ASTMD790 | 110 MPa |
| | ASTMD1044 | 200 mg |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD412 | 16.5 MPa |
elongation | | ASTMD412 | 250 % |
tear strength | | ASTMD624 | 78.8 kN/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD696 | 1.4E-04 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.