PA46 Stanyl® TS300MB
149
- Properties:Thermal stabilityFlame retardant
- Usages:CastersFitness equipmentFoamFootwear
Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ISO 294-4 | 1.3 % | |
Water absorption rate | ISO 62 | 2.6 % | |
density | ISO 1183 | 1.41 g/cm³ |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO 180-1A | 21 kJ/m² | |
Impact strength of cantilever beam gap | ISO 180-1A | 21 kJ/m² | |
tensile strength | ISO 527-2 | 110 Mpa | |
ISO 527-2 | 100 Mpa | ||
Tensile modulus | ISO 527-2 | 5500 Mpa | |
ISO 527-2 | 5000 Mpa | ||
Flexural modulus | ISO 178 | 4700 Mpa | |
ISO 178 | 3900 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+11 ohm*cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melting temperature | ISO 3146 | 295 °C | |
Heat distortion temperature | ISO 75-1 | 290 °C | |
Linear coefficient of thermal expansion | ISO 11359-2 | 0.00002 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.