Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 0.918 g/cm³ | |
melt mass-flow rate | ASTM D1238 | 2.0 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
gloss | ASTM D2457 | 92 | |
Haze ratio | ISO 14782 | 1.8 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Elmendorf tear strength | ISO 6383-2 | 190 N | |
film thickness | 20 µm | ||
Tensile modulus | ISO 178 | 165 MPa | |
ISO 178 | 170 MPa | ||
tensile strength | ISO 527-3 | 9.70 MPa | |
ISO 527-3 | 9.60 MPa | ||
ISO 527-3 | 37.0 MPa | ||
ISO 527-3 | 23.0 MPa | ||
elongation | ISO 527-3 | 330 % | |
ISO 527-3 | 670 % | ||
Dart impact | ISO 7765-1 | 35 g | |
Elmendorf tear strength | ISO 6383-2 | 12 N |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM D15253 | 100 °C | |
melting temperature | 内部方法 | 121 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.