Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.06 g/cm³ |
pH value | | | 7.0to9.0 |
Solid Content | | | 39to41 % |
thermosetting | Test Condition | Test Method | Test Result |
---|
Thermosetting mixed viscosity | | | 40.0to100 cP |
hardness | Test Condition | Test Method | Test Result |
---|
Hardness | | | HB-B |
Shore hardness | | | 10.0 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
Cosolvent-N-Methylpyrrolidone | | | 2.6 % |
Minimum Film Forming Temperature | | | 0 °C |
elastomer | Test Condition | Test Method | Test Result |
---|
tensile strength | | | 4.83 MPa |
tensile strength | | | 34.5 MPa |
elongation | Break | | 550 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | | -46.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.