Technical Data Sheet
Test Condition | Test Method | Test Result | |
---|---|---|---|
Shrinkage rate | ISO 2577 | 0.60to1.2 % | |
Water absorption rate | ASTM D570 | 0.080 % | |
ISO 62 | 0.080 % | ||
tensile strength | Yield | ASTM D638 | 74.0 MPa |
bending strength | ISO 178 | 90.0 MPa | |
Impact strength of cantilever beam gap | ASTM D256 | 49 J/m | |
ISO 180/1A | 4.0 kJ/m² | ||
tensile strength | Yield | ISO 527-2/5 | 70.0 MPa |
elongation | Break | ASTM D638 | 4.0 % |
Tensile strain | Break | ISO 527-2/5 | 4.0 % |
Flexural modulus | ASTM D790 | 3900 MPa | |
ISO 178 | 3500 MPa | ||
bending strength | ASTM D790 | 98.0 MPa | |
UL flame retardant rating | UL 94 | V-0 | |
Rockwell hardness | R-Scale | ASTM D785 | 113 |
R-Scale | ISO 2039-2 | 113 | |
Heat distortion temperature | ASTM D648 | 135 °C | |
ISO 75-2/A | 125 °C | ||
vicat | ISO 306/B50 | 147 °C | |
ISO 306/B120 | 151 °C | ||
UL flame retardant rating | UL 94 | V-0 | |
density | ASTM D792 | 1.45 g/cm³ | |
ISO 1183 | 1.45 g/cm³ | ||
melt mass-flow rate | ASTM D1238 | 30 g/10min | |
ISO 1133 | 30 g/10min | ||
Shrinkage rate | ASTM D955 | 0.60to1.2 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.