Share
Add to compare

PUR-Ether//TDI 89-LC USA Anderson Development

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

elastomerTest ConditionTest MethodTest ResultTest Unit
tensile strength100%StrainASTM D4123.17MPa
tensile strength300%StrainASTM D4124.83MPa
tensile strengthYieldASTM D41222.8MPa
elongationBreakASTM D412730%
Shore hardnessASTM D263273%
thermosettingTest ConditionTest MethodTest ResultTest Unit
storage stability0.75to1.0min
stripping time100°C8.0min
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreAASTM D224070
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.