physical property | Test Condition | Test Method | Test Result |
---|
colour | | | 1.2到1.7 |
density | | ASTMD792 | 1.75到1.85 g/cm³ |
Tightening rate | | ASTMD1895 | 1.5到2.0 |
Shrinkage rate | | ASTMD955 | 0.050到0.15 % |
Water absorption rate | | ASTMD570 | 0.12 % |
colour | | | 1.0到1.5 |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 45到55 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-0 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Compression Modulus | | ASTMD695 | 345000到379000 MPa |
compressive strength | | ASTMD695 | 96.5到110 MPa |
shear strength | | ASTMD732 | 55.2到62.1 MPa |
tensile strength | | ASTMD638 | 41.4到62.1 MPa |
Flexural modulus | | ASTMD790 | 12400到13100 MPa |
bending strength | | ASTMD790 | 124到145 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 430到750 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTMD149 | >14 kV/mm |
arc resistance | | ASTMD495 | >185 sec |
Inclined-PlaneTracking | | ASTMD2303 | >1000 min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | >260 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.