POM CH-20 JAPAN POLYPLASTIC
180
Form:Granules | Grade:Enhanced level
Properties:
wear resistantCarbon fiber reinforcedConductiveWeather resistanceThermal stabilityFiller: Carbon fiber rein20%Filler by weight
Typical Applications:
Automotive sectorBottle capFiber grade
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Automotive sector | Bottle cap | Fiber grade |
| Properties: | wear resistant | Carbon fiber reinforced | Conductive | Weather resistance | Thermal stability | Filler: Carbon fiber rein | 20% | Filler by weight |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.0 | kJ/m² |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Friction coefficient | Steel - Dynamic3 | JISK7218 | 0.24 | |
| Wear factor | 0.49MPa,0.30m/sec4 | JISK7218 | 5.0 | 10^-8mm³/N·m |
| 0.060MPa,0.15m/sec5 | JISK7218 | 50 | 10^-8mm³/N·m | |
| 0.49MPa,0.30m/sec6 | JISK7218 | 300 | 10^-8mm³/N·m | |
| 0.060MPa,0.15m/sec7 | JISK7218 | 10000 | 10^-8mm³/N·m | |
| Tensile modulus | ISO 527-2 | 14000 | Mpa | |
| tensile strength | ISO 527-2 | 144 | Mpa | |
| Tensile strain | Break | ISO 527-2 | 1.5 | % |
| Bending modulus | ISO 178 | 12000 | Mpa | |
| bending strength | ISO 178 | 205 | Mpa | |
| Friction coefficient | Dynamic2 | JISK7218 | 0.35 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 163 | °C |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 1E-05 | cm/cm/°C |
| TD:23to55°C | Internal Method | 8E-05 | cm/cm/°C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183 | 1.47 | g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 2.5 | g/10min |
| Melt Volume Flow Rate (MVR) | 190°C/2.16kg | ISO 1133 | 2.00 | cm3/10min |
| Shrinkage rate | TD:2.00mm | ISO 294-4 | 0.80 | % |
| MD:2.00mm | ISO 294-4 | 0.30 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | 50 | ohms | |
| Volume resistivity | IEC 60093 | 1E+02 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Scale | ISO 2039-2 | 95 | |
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| ColourNumber | CD3501 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.