Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO 1183/D | 0.920 g/cm³ |
melt mass-flow rate | | ISO 1133 | 2.0 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTM D2457 | 45 |
transparency | | ASTM D1746 | 50.0 |
Haze ratio | | ASTM D1003 | 17 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
coefficient of friction | | BS2782 | 0.11 |
film | Test Condition | Test Method | Test Result |
---|
Dart impact | | ISO 7765-1/A | 80 g |
tensile strength | | ISO 1184 | 10.0 MPa |
tensile strength | | ISO 1184 | 11.0 MPa |
elongation | | ISO 1184 | 850 % |
elongation | | ISO 1184 | 950 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ISO 306 | 100 °C |
melting temperature | | ISO 3146 | 121 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.