Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
Thermosetting components | Resin | | 100 |
Thermosetting components | Hardener | | 按重量计算的混合比:9.0 |
Post curing time | | | 170 hr |
Post curing time | | | 16 hr |
Uncured Properties | Test Condition | Test Method | Test Result |
---|
Curing Time | | | 1.0 hr |
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.11 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | Shore A | ASTM D2240 | 95 |
elastomer | Test Condition | Test Method | Test Result |
---|
tear strength | Split | ASTM D470 | 27 kN/m |
compression set | | ASTM D395B | 30 % |
Shore hardness | | ASTM D2632 | 60 % |
tensile strength | | ASTM D412 | 9.27 MPa |
tensile strength | | ASTM D412 | 18.2 MPa |
tensile strength | | ASTM D412 | 37.6 MPa |
elongation | Break | ASTM D412 | 460 % |
tear strength | | ASTM D624 | 123 kN/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.