Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ISO294-4 | 0.70到1.0 % |
Shrinkage rate | | ISO294-4 | 0.75到1.0 % |
Water absorption rate | | ISO62 | 0.050 % |
density | | ISO1183 | 1.32 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|
Hot filament ignition temperature | | IEC60695-2-13 | 750 °C |
Limiting Oxygen Index | | ASTMD2863 | 26 % |
UL flame retardant rating | | UL94 | V-0 |
UL flame retardant rating | | UL94 | V-0 |
UL flame retardant rating | | UL94 | V-0 |
Burning wire flammability index | | IEC60695-2-12 | 960 °C |
Burning wire flammability index | | IEC60695-2-12 | 960 °C |
Hot filament ignition temperature | | IEC60695-2-13 | 750 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile strain | | ISO527-2/5 | 6.5 % |
Tensile strain | | ISO527-2/5 | 8.0 % |
Tensile strain | | ISO527-2/5 | 12 % |
Tensile strain | | ISO527-2/5 | 20 % |
Tensile stress | | ISO527-2/5 | 10.0 MPa |
Tensile stress | | ISO527-2/5 | 7.00 MPa |
Tensile strain | | ISO527-2/5 | 2.5 % |
Tensile strain | | ISO527-2/5 | 6.0 % |
Tensile modulus | | ISO527-2/1 | 3200 MPa |
Tensile stress | | ISO527-2/5 | 25.0 MPa |
Tensile stress | | ISO527-2/5 | 20.0 MPa |
Tensile stress | | ISO527-2/5 | 10.0 MPa |
Tensile stress | | ISO527-2/5 | 15.0 MPa |
Tensile modulus | | ISO527-2/1 | 1400 MPa |
Tensile modulus | | ISO527-2/1 | 950 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO179/1eA | 2.4 kJ/m² |
Charpy Notched Impact Strength | | ISO179/1eA | 5.0 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 8.0 kJ/m² |
Impact strength of simply supported beam without notch | | ISO179/1eU | 25 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
CTI | | IEC60112 | 600 V |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO75-2/B | 120 °C |
| | ISO75-2/A | 60.0 °C |
| | | 105 °C |
vicat | | ISO306/B50 | 75.0 °C |
| | ISO11359-2 | 3.5E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.