Test Condition | Test Method | Test Result | |
---|---|---|---|
线性热膨胀系数 | MD:20到100°C | ASTMD696 | 1.2E-04 cm/cm/°C |
比热 | 1050 J/kg/°C | ||
导热系数 | ASTMC177 | 0.26 W/m/K | |
UL阻燃等级 | 1.6mm | UL94 | V-0 |
极限氧指数 | 1.57mm | ASTMD2863 | >95 % |
熔体粘度 | 380°C | 2.00E+6到2.50E+7 mPa·s | |
密度 | ASTMD792 | 2.14到2.16 g/cm³ | |
表观密度 | JISK6891 | 1.00到1.40 g/cm³ | |
熔体质量流动速率 | 372°C/5.0kg | ASTMD1238 | 20到30 g/10min |
吸水率 | Saturation | ASTMD570 | <0.010 % |
熔融温度 | ASTMD4591 | 300到310 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.