Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.84 g/cm³ |
Water absorption rate | | ASTMD570 | 0.23 % |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 45到50 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ASTMD790 | 6150 MPa |
Flexural modulus | | ASTMD790 | 15300 MPa |
Flexural modulus | | ASTMD790 | 16200 MPa |
Flexural modulus | | ASTMD790 | 7130 MPa |
Flexural modulus | | ASTMD790 | 7960 MPa |
Flexural modulus | | ASTMD790 | 6800 MPa |
bending strength | | ASTMD790 | 223 MPa |
bending strength | | ASTMD790 | 238 MPa |
bending strength | | ASTMD790 | 73.5 MPa |
bending strength | | ASTMD790 | 77.5 MPa |
bending strength | | ASTMD790 | 47.0 MPa |
bending strength | | ASTMD790 | 50.0 MPa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | ASTMD257 | 1.0E+6到1.0E+10 ohms |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | 内部方法 | 1.3E-05 cm/cm/°C |
specific heat | | ASTME1269 | 946 J/kg/°C |
thermal conductivity | | ASTME1925 | 0.43 W/m/K |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.