PA6 GFR 50 NATURAL

0
  • Properties:
    Glass fiber reinforced material
    50%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Water absorption rateISO 620.20 %
densityISO 11831.54 to 1.56 g/cm³
Shrinkage rateISO 294-40.30 %
Shrinkage rate0.20
ash contentISO 345149 to 51 %
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ISO 527-2230 to 250 MPa
Tensile strainISO 527-22.0 to 3.0 %
Hardness (Shore)ISO 86887 to 90
Tensile modulusISO 527-216000 to 17500 MPa
Flexural modulusISO 17813000 to 15000 MPa
bending strengthISO 178280 to 310 MPa
Charpy Notched Impact StrengthISO 179/1eA16 to 22 kJ/m²
Impact strength of cantilever beam gapISO 180/1A16 to 22 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature (HDT)ISO 75-2/A215
vicatISO 306/B215
melting temperatureISO 3146215 to 225
UL flame retardant ratingUL 94HB
Hot deformation temperature (HDT)ISO 75-2/B225
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.