PPS PPS-hGR40
30
- Properties:enhance
- Usages:AerospacemachineMechanical componentsElectrical fieldElectronic fieldElectrical appliances
- Certificates:UL
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | Internal Method | 1.70 g/cm³ | |
Shrinkage rate | Internal Method | 0.25 % | |
Internal Method | 0.75 % | ||
Rockwell hardness 2 | Internal Method | 110 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Internal Method | 180 Mpa | |
elongation | Internal Method | 2.8 % | |
Flexural modulus | Internal Method | 13600 Mpa | |
bending strength | Internal Method | 272 Mpa | |
compressive strength | Internal Method | 130 Mpa | |
Impact strength of cantilever beam gap | Internal Method | 14 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | Internal Method | 265 °C | |
melting temperature | Internal Method | 288 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.