Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.10 g/cm³ |
Water absorption rate | | ASTMD570 | 0.20 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 90到100 |
Barcol Hardness | | ASTMD2583 | 48到52 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
CyclesFreeze-Thaw- | | 内部方法 | NoEffect |
HotFormingTemperature | | 内部方法 | 149到171 °C |
HotFormingTemperature | | 内部方法 | 177到193 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ASTMD790 | 61.4 MPa |
bending strength | | ASTMD790 | 73.8 MPa |
Tensile modulus | | ASTMD638 | 2410 MPa |
tensile strength | | ASTMD638 | 42.1 MPa |
elongation | | ASTMD638 | 6.2 % |
Flexural modulus | | ASTMD790 | 2310 MPa |
Flexural modulus | | ASTMD790 | 2230 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256A | 170 J/m |
Dart impact equipped with measuring instruments | | 内部方法 | 73.2 J |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 89.4 °C |
| | ASTMD696 | 7.7E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.