PUR-Ester LF 1900A CHEMTURU USA

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.27 g/cm³
thermosettingTest ConditionTest MethodTest Result
STORAGE STABILITY6.0to8.0 min
stripping time30to45 min
Uncured PropertiesTest ConditionTest MethodTest Result
Curing Time16 hr
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224090to93
Mechanical propertiesTest ConditionTest MethodTest Result
compressive strengthASTM D6951.65 MPa
compressive strengthASTM D6952.62 MPa
compressive strengthASTM D6953.62 MPa
compressive strengthASTM D6954.96 MPa
compressive strengthASTM D6956.69 MPa
elastomerTest ConditionTest MethodTest Result
elongationBreakASTM D412530 %
tear strengthASTM D624105 kN/m
tear strengthSplitASTM D47024 kN/m
compression setASTM D395B32 %
Shore hardnessASTM D263227 %
tensile strength ASTM D4128.27 MPa
tensile strength ASTM D41210.3 MPa
tensile strength ASTM D41215.2 MPa
tensile strength ASTM D41249.6 MPa
filmTest ConditionTest MethodTest Result
Tear resistance of pantsASTM D193847.3 N/mm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.