Share
Add to compare

Polyester, TS UP 804 Hexion Inc.

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Charpy Notched Impact Strength23°CISO 179/1eA4.0kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU7.0kJ/m²
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.5mmUL 94V-1
UL flame retardant rating1.4mmUL 94V-0
UL flame retardant rating1.5mmUL 94V-0
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Bending modulusISO 17815000MPa
bending strengthISO 178105MPa
Compressive stressISO 604250MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature8.0MPa,UnannealedISO 75-2/C205°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
density23°CISO 11832.10g/cm³
Apparent densityISO 600.92g/cm³
Shrinkage rateISO 25770.13%
Water absorption rateISO 6213.0mg
Shrinkage rateISO 25770.010%
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Compared to the anti leakage trace indexSolutionAIEC 60112PLC 0
Surface resistivityIEC 600931E+12ohms
Volume resistivityIEC 600931E+13ohms·cm
Dielectric strength1.00mmIEC 60243-128kV/mm
Relative permittivity100HzIEC 602505.50
Dissipation factor100HzIEC 602500.010
hardnessTest ConditionTest MethodTest ResultTest Unit
Ball Pressure TestH961/30ISO 2039-1425MPa
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
Compression molding pressure>15.0MPa
Compression molding temperature160to190°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.