TPU D125K HC

0
  • Properties:
    Conductivity
    low speed solidification point

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D-7921.20 g/cm³
Shore hardnessShore AASTM D-224095
Wear amountDIN 53516110 mm³
squeeze outTest ConditionTest MethodTest Result
drying temperature90.0 to 100
drying time2.0 hr
elastomerTest ConditionTest MethodTest Result
tensile strength ASTM D-41210.0 MPa
tensile strength YieldASTM D-41212.0 MPa
elongationBreakASTM D-412500 %
Electrical performanceTest ConditionTest MethodTest Result
Surface Resistivity内部方法< 1.0E+3 ohms
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureDIN 51007-35.0
melting temperature内部方法> 180
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.