TPU-Ester RTP 1201-80D

0
  • Properties:
    Filler
    glass fiber reinforced material
    10%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.29 g/cm³
Shrinkage rateASTMD9550.50 %
Water absorption rateASTMD5700.20 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTMD785114
ASTMD224083
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL94HB
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD6384140 MPa
tensile strengthYieldASTMD63865.5 MPa
elongationBreakASTMD6388.0 %
Flexural modulusASTMD7903100 MPa
bending strengthYieldASTMD790103 MPa
compressive strengthASTMD69548.3 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD25669 J/m
Suspended wall beam without notch impact strengthASTMD4812430 J/m
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTMD2571E+11 ohms·cm
dielectric strengthASTMD14918 kV/mm
dielectric constantASTMD1505.00
Dissipation FactorASTMD1500.011
arc resistanceASTMD49590.0 sec
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648104 °C
ASTMD64865.6 °C
ASTMD6961.3E-04 cm/cm/°C
thermal conductivityASTMC1770.26 W/m/K
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.