LDPE ExxonMobil™ HP20023
26
- Properties:No additivesHigh mobility
- Usages:SealsColor masterbatch carrier
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | ASTM D1238 | 20 g/10 min | |
Environmental stress cracking resistance | ASTM D1693B | 2.00 hr | |
ASTM D1693B | 6.00 hr |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ISO 868 | 45 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTM D638 | 225 Mpa | |
tensile strength | ASTM D638 | 8.00 Mpa | |
ASTM D638 | 9.00 Mpa | ||
elongation | ASTM D638 | 150 % | |
Flexural modulus | ASTM D790 | 175 Mpa | |
bending strength | ASTM D790 | 7.00 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Suspended wall beam without notch impact strength | ASTM D256 | 500 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM D1525 | 92.0 °C | |
melting temperature | 内部方法 | 112 °C | |
Crystallization peak temperature | ISO 11357-3 | 98 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.