| optical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| turbidity | 40.0μm,Blown Film | ASTM D1003 | 13 % |
| gloss | 45°,40.0μm,Blown Film | ASTM D2457 | 50 |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Friction coefficient | Itself - Dynamic,Blown Film | ISO 8295 | >0.40 |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Vicat softening temperature | ISO 306/A | 96.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 0.25 g/10min |
| film | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Elmendorf tear strength | TD:40μm,Blown Film | ISO 6383-2 | 9.3 N |
| MD:40μm,Blown Film | ISO 6383-2 | 5.8 N | |
| Dart impact | 40μm,Blown Film | ISO 7765-1 | 950 g |
| elongation | TD:Break,40μm,Blown Film | ISO 527-3 | 520 % |
| MD:Break,40μm,Blown Film | ISO 527-3 | 480 % | |
| tensile strength | TD:Break,40μm,Blown Film | ISO 527-3 | 20.0 Mpa |
| MD:Break,40μm,Blown Film | ISO 527-3 | 21.0 Mpa | |
| film thickness | 40 µm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.