PPO APS130-7002 SABIC INNOVATIVE US
133
Form:Granules
Properties:
Thermal stabilityGlass fiber reinforcedFiller: Glass fiber reinf30%Filler by weight
Typical Applications:
medical care
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | medical care |
| Properties: | Thermal stability | Glass fiber reinforced | Filler: Glass fiber reinf | 30% | Filler by weight |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| bending strength | ASTM D790 | 157 | Mpa | |
| Bending modulus | ASTM D790 | 8430 | Mpa | |
| elongation | Break | Internal Method | 8.0 | % |
| tensile strength | Yield | Internal Method | 113 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 267 | °C |
| Linear coefficient of thermal expansion | MD:-30to30°C | ASTME831 | 2.5E-5到5.5E-5 | cm/cm/°C |
| Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTM D648 | 267 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 24hr | ASTM D570 | 0.020 | % |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.25-0.70 | % |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 29 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 60Hz | ASTM D150 | 3.30 | |
| 50Hz | ASTM D150 | 3.30 | ||
| Dielectric strength | 1.60mm,inOil | ASTM D149 | 22 | KV/mm |
| Surface resistivity | ASTM D257 | 1E+16 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.